Inconel 600 Chemical Composition Limits

Inconel 600 Chemical Composition Limits

Weight%

C

S

Cr

Cu

Mn

Si

Ni

Fe

Nickel Alloy 600

0.15 max

0.015 max

14.0 - 17.0

0.50 max

1.0 max

0.50 max

72.0 min

6 - 10


Inconel 600 Mechanical Properties

Material

Form and Condition

Tensile Strength

Yield Strength

Elongation %

Hardness, Rockwell

ksi

MPa

ksi

MPa

Alloy 600 rod and bar

Cold drawn Annealed

80-100

550-690

25-50

170-345

55-35

65-85B

Alloy 600 Plate

Hot rolled Annealed

80-100

550-725

30-50

205-345

55-35

65-85B

Alloy 600 Sheet

Cold Rolled Annealed

80-100

550-690

30-45

205-310

55-35

88B max

Alloy 600 Tube and Pipe

Cold Drawn Annealed

80-100

550-690

25-50

170-345

55-35

88B max

Alloy 600 Wire

Cold Drawn Annealed

80-120

550-830

35-75

240-520

45-20

-

Alloy 600 Wire

Cold Drawn No 1 Temper

105-135

725-930

70-105

480-725

35-15

-

Alloy 600 Wire

Spring Temper

170-220

1170-1520

150-210

1035-1450

5-2

-

JACKY WINN
G.M.
PETROL STEEL CO., LTD
T:+ 86(0) 10 8599 9168
Mo. + 86 159 0035 7871
www.petrosteels.com
www.sinosuperalloy.com


Known as one of the professional manufacturers and suppliers of quality steel products, Petrol Steel Co.,Ltd is always at your service. Should you are interested in our Inconel 600, you can check the mechanical properties, medical composition, hardness value and even the melting point with us first if you need. Now wholesale Inconel 600 in stock with our factory!

Hot Tags: Inconel 600 manufacturers, suppliers, factory, wholesale, in stock, melting point, mechanical properties, chemical composition, hardness value

Related Products

Feedback

We're Here to Help

  • +86 159 0035 7871

    +86 159 0035 7871

    JACKYWINN@FOXMAIL.COM

     A-4F, Wantone Center, A6, Chaowai St., Chaoyang Dist., Beijing, China

Newsletter

Enter in your email address to receive deals
and coupons.
Bookmark us today!