Therere are available Inconel 718 material stocks in our factory Inconel 718 (UNS N07718) is available in Wire, Billet, Strip, Rod, Sheet, Plate, Forging Stock and Welding Wire. For all stock availability contact Sales. Specifications

Description

Inconel 718 (UNS N07718, W Nr 2.4668) is an austenitic nickel-based superalloy. Alloy 718 exhibits excellent high yield tensile and creep-rupture properties at temperatures up to 1300oF and oxidation resistance to 1800oF. Alloy 718 is used in applications that require high strength such as parts for jet engines and high speed airframe parts such as wheels, buckets, spacers and high temperature bolts and fasteners.


Specifications

UNS N07718

Werkstoff Nr 2.4668

AMS 5596 Sheet, Strip and Plate

AMS 5597 Sheet, Strip and Plate

ASTM B637 Forgings

ASTM B670 Plate, Sheet and Strip

AFNOR NC 19 Fe Nb,

MSRR 7115 and MSRR 7116

Inconel 718 (trademark)

FMC Spec M40110, M40118, M40125, M40902, M40908, M40909, M40910

NACE MR-0175/ISO 15156


Inconel 718 (UNS N07718) is available in Rod,Rings,Forgings,pipe,tube,bars,plates,sheets,Strip, wire, Billet, Forging Stock and Welding Wire. For all stock availability contact Sales.

Known as one of the professional manufacturers and suppliers of quality steel products, Petrol Steel Co.,Ltd is always at your service. Should you are interested in our Inconel 718 material stocks in our factory, you can check the mechanical properties, medical composition, hardness value and even the melting point with us first if you need. Now wholesale Inconel 718 material stocks in our factory in stock with our factory!

Hot Tags: Inconel 718 material stocks in our factory manufacturers, suppliers, factory, wholesale, in stock, melting point, mechanical properties, chemical composition, hardness value

Related Products

Feedback

We're Here to Help

  • +86 159 0035 7871

    +86 159 0035 7871

    JACKYWINN@FOXMAIL.COM

     A-4F, Wantone Center, A6, Chaowai St., Chaoyang Dist., Beijing, China

Newsletter

Enter in your email address to receive deals
and coupons.
Bookmark us today!