Inconel 625 (UNS N06625) is a nickel-chromium-molybdenum alloy with an addition of niobium. The addition of molybdenum acts with the niobium to stiffen the alloy matrix, providing a high strength without a strengthening heat treatment.

Description

Inconel 625 (UNS N06625) is a nickel-chromium-molybdenum alloy with an addition of niobium. The addition of molybdenum acts with the niobium to stiffen the alloy matrix, providing a high strength without a strengthening heat treatment. The alloy resists a wide range of corrosive environments and has a good resistance to pitting and crevice corrosion. Inconel 625 is used in chemical processing, aerospace and marine engineering oil & gas, pollution control equipment and nuclear reactors.

Inconel 625 Chemical Composition Limits

Weight %

Ni

Cr

Mo

Nb + Ta

Fe

Ti

C

Mn

Si

S

P

Al

Co

Alloy 625

58.0 min

20 - 23

8 -10

3.15 -4.15

5.0 max

0.40 max

0.10 max

0.50 max

0.50 max

0.15 max

0.15 max

0.40 max

1.0 max

Inconel 625 Mechanical Properties

Material

Form and Condition

Tensile Strength MPa

Yield Strength (0.2% Offset) MPa

Elongation 4D(%)

Hardness HB

Ksi

MPa

Ksi

MPa

Alloy 625 Bar

Annealed

120

827

60

414

30

≤ 287 HB

Alloy 625 Sheet

Annealed

120

827

60

414

30

145-240

Alloy 625 Tube
Seamless and Welded

Annealed

120

827

60

414

35

-

JACKY WINN
G.M.
PETROL STEEL CO., LTD
T:+ 86(0) 10 8599 9168
Mo. + 86 159 0035 7871
www.petrosteels.com
www.sinosuperalloy.com


Known as one of the professional manufacturers and suppliers of quality steel products, Petrol Steel Co.,Ltd is always at your service. Should you are interested in our superalloy Inconel 625, you can check the mechanical properties, medical composition, hardness value and even the melting point with us first if you need. Now wholesale superalloy Inconel 625 in stock with our factory!

Hot Tags: superalloy Inconel 625 manufacturers, suppliers, factory, wholesale, in stock, melting point, mechanical properties, chemical composition, hardness value

Related Products

Feedback

We're Here to Help

  • +86 159 0035 7871

    +86 159 0035 7871

    JACKYWINN@FOXMAIL.COM

     A-4F, Wantone Center, A6, Chaowai St., Chaoyang Dist., Beijing, China

Newsletter

Enter in your email address to receive deals
and coupons.
Bookmark us today!