Superior Inconel 718 3D Printing Spherical Powder Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods

Inconel 718 (UNS N07718, W Nr 2.4668) is an austenitic nickel-based superalloy. Alloy 718 exhibits excellent high yield tensile and creep-rupture properties at temperatures up to 1300ºF and oxidation resistance to 1800ºF. Alloy 718 is used in applications that require high strength such as parts for jet engines and high speed airframe parts such as wheels, buckets, spacers and high temperature bolts and fasteners.

Description


Superior Inconel 718 3D Printing Spherical Powder Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods


We are leading manufacturer and stockiest of Inconel 718 in China.


Inconel 718 Chemical Composition Limits

Weight %

C

Mn

P

S

Si

Cr

Ni

Mo

Cb

Ta

Ti

Al

Co

B

Cu

Fe

Alloy 718
   
AMS 5662

0.08

0.35

0.015

0.015

0.35

17-21

50-55

2.8-3.30

4.75-5.50

0.05

0.65-1.15

0.20-0.80

1.00

0.006

0.30

Rem

Inconel 718 (UNS N07718, W Nr 2.4668) is an austenitic nickel-based superalloy. Alloy 718 exhibits excellent high yield tensile and creep-rupture properties at temperatures up to 1300ºF and oxidation resistance to 1800ºF. Alloy 718 is used in applications that require high strength such as parts for jet engines and high speed airframe parts such as wheels, buckets, spacers and high temperature bolts and fasteners.
This is the preferred treatment in tensile-limited applications as it produces the best transverse ductility in heavy sections, impact strength and low temperature notch tensile strength. However, this treatment has a tendency to produce notch brittleness in stress rupture.


Material

Condition

Tensile Strength
     ksi

Yield Strength
     ksi

Elongation
     4D

Reduction of Area
     %

Hardness

AMS 5662 Bar

1700-1850°F Anneal

-

-

-

-

≤ 277 HB

AMS 5663 Bar

1700-1850°F Anneal + Age

185

150

12

15

≥331 HB

AMS 5664 Bar

1900-1950°F Anneal

-

-

-

-

3" dia 248 HB
     3-5" dia 285 HB


1900-1950°F Anneal + Age

180

150

10

12

≥341 HB

Typical Mechanical Properties of Inconel 718 Bar above and Alloy 718 Sheet below.

Material

Condition

Tensile Strength
     ksi

Yield Strength
     ksi

Elongation
     4D

Hardness

Alloy 718 Sheet

AMS 5596 < 0.1874" thick

140

80

30

102 HRB

Alloy 718 Sheet

AMS 5596 Aged < 0.1874" thick

180

150

12

≥36 HRC

Alloy 718 Sheet

AMS 5597

140

75

30

≤ 25 HRC

Alloy 718 Sheet

AMS 5597 + Aged

180

150

15

≥38 HRC

Availability

Inconel 718 (UNS N07718) is available in Wire, Billet, Strip, Rod, Sheet, Plate, Forging Stock and Welding Wire. For all stock availability contact Sales.
Specifications
UNS N07718
Werkstoff Nr 2.4668
AMS 5596 Sheet, Strip and Plate
AMS 5597 Sheet, Strip and Plate
ASTM B637 Forgings
ASTM B670 Plate, Sheet and Strip
AFNOR NC 19 Fe Nb,
MSRR 7115 and MSRR 7116
Inconel 718 (trademark)
FMC Spec M40110, M40118, M40125, M40902, M40908, M40909, M40910
NACE MR-0175/ISO 15156


The Inconel 718 items which we can manufacture and supply are the followings.
3D printing spherical powder Inconel 718
Inconel 718 Rings, Forgings, pipe, tube, bars, plates, sheets, Strip, wire, fitting Union, Pipe Elbows, PIPE Tee, ADAPTERS, pipe bend, reducers, fitting caps, pipe outlets, Stub Ends, Couplings, pipe Nipples, BUSHINGS, pipes sockets, Pipe Gasket, pipe joints, pipe Cross, Pipe Wyes, seal ring, Flange, bolts, nuts, Rod


ONE OF THE KIND, MILLIONS OF CHOICES
SUPERIOR QUALITY
PROMPT DELIVERY
FAVORABLE FEEDBACK
ALL AVAILABLE IN PESCO
SELECT PESCO, YOU WILL BE RIGHT


For more info and price of Inconel 718, please send us inquiry and you will have quick reply soon.

Known as one of the professional manufacturers and suppliers of quality steel products, Petrol Steel Co.,Ltd is always at your service. Should you are interested in our Superior Inconel 718 3D Printing Spherical Powder Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods, you can check the mechanical properties, medical composition, hardness value and even the melting point with us first if you need. Now wholesale Superior Inconel 718 3D Printing Spherical Powder Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods in stock with our factory!

Hot Tags: Superior Inconel 718 3D Printing Spherical Powder Forgings Pipes Tubes Bars Plates Sheets Strips Wires Rods manufacturers, suppliers, factory, wholesale, in stock, melting point, mechanical properties, chemical composition, hardness value, inconel 718

Related Products

Feedback

We're Here to Help

  • +86 159 0035 7871

    +86 159 0035 7871

    JACKYWINN@FOXMAIL.COM

     A-4F, Wantone Center, A6, Chaowai St., Chaoyang Dist., Beijing, China

Newsletter

Enter in your email address to receive deals
and coupons.
Bookmark us today!